MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik SILIKOFTAL® HTL 2 Silicone Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS; Silicone

Material Notes: Special features:
  • low yellowing
  • good adhesion
  • without addition of organotin-containing compounds
  • minimal thermoplasticity
Application:
  • non-stick coatings in combination with PTFE
  • decorative coatings of cookware, household appliances and electric and gas heaters with a permanent thermal stability of 220 °C

      Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 40 %40 %
Viscosity 1200 cP1200 cP
 
Descriptive Properties
Appearanceclear to slightly hazy liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik SILIKOFTAL® HTL 3 Silicone Polyester Resin
Evonik SILIKOFTAL® HTT Silicone Polyester Resin
Evonik SILIKOFTAL® HTF MPA/MBA Silicone Polyester Resin
Evonik SILIKOFTAL® HTF Silicone Polyester Resin
BASF Luwax® OA 5 Pastilles/Powder

PEVONIL425 / 196629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.