MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AGC Fluon® FC123 PTFE, 15% Graphite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Fluon® FC 123 (310 123 071) is a 15% graphite-filled, PTFE product designed for use in large billet molding. This compound is supplied dry powder form.

End Uses: Graphite powder is added to PTFE to improve the lubricity and wear properties of PTFE especially against soft metals.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.13 g/cc2.13 g/ccASTM D4745
Filler Content 15 %15 %ASTM D4745
Deformation 5.7 %5.7 %Under Load
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959Sustained; ASTM D2240
 6161Peak; ASTM D2240
Tensile Strength 21.4 MPa3100 psiASTM D4745
Elongation at Break 200 %200 %ASTM D4745
Coefficient of Friction, Dynamic 0.0700.070ASTM D3702
K (wear) Factor 60.4 x 10-8 mm³/N-M30.0 x 10-10 in³-min/ft-lb-hr5000 PV; ASTM D3702

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
AGC Fluon® FC 103 PTFE, 15% Glass Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
AGC FC 423 PTFE, 15% Graphite
AGC FC 123 PTFE, 15% Graphite

PAGCX127 / 191236

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.