MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Loctite® 5072 Silicone Chip Coating
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes:
Conformal Coatings
Conformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Loctite offers both acrylic/urethane and silicone conformal coatings which are cured by UV, heat, or a two-part cure mechanism.

Loctite® 5072 Silicone Chip Coating
This gel, UV curable silicone chip coating, is a soft, low ionic material for coating bare silicon die. Cure Type: UV

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 2900 cP2900 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 7272
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 3.50e+16 ohm>= 3.50e+16 ohmASTM D257
Dielectric Strength 17.7 kV/mm450 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 min0.0167 hourUV Full Cure in 60 seconds at 75 mW/cm^2
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
Resinlab® EP1385 Clear Epoxy Formulation
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Henkel Loctite® 3532 High viscosity Dam Encapsulant

PLOCT178 / 51914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.