MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: 8.9 wt% Vinyl Acetate.

Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

General Processing Information: Resin melt temperature should be maintained in the range 150-175°C (300-350°F) to provide a suitable viscosity for blown film extrusion. Selection of a specific melt temperature will depend on considerations such as desired gauge, height of tower or cooling capacity, optical properties and winder and other machine variables. Excessively high melt temperatures, above 230°C (450°F) may cause thermal degradation of the resin.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
Moisture Vapor Transmission 0.630 cc-mm/m²-24hr-atm1.60 cc-mil/100 in²-24hr-atmg-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
Oxygen Transmission 197 cc-mm/m²-24hr-atm
@Thickness 0.0254 mm
500 cc-mil/100 in²-24hr-atm
@Thickness 0.00100 in
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
Melt Flow 2.0 g/10 min2.0 g/10 minCondition not noted.; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 %550 %MD-TD Average; ASTM D882
Film Elongation at Break, TD 550 %550 %MD-TD Average; ASTM D882
Impact 22.722.7J/mm Spencer Impact; Average of MD and TD; ASTM D3420
Elmendorf Tear Strength, MD 3.31 g/micron84.0 g/milAverage of MD and TD; ASTM D1922
Film Tensile Strength at Break, MD 24.8 MPa3600 psiMD-TD Average; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 81.0 °C178 °FFreezing Point via DSC/ASTM D3418
 101 °C214 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 83.0 °C181 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %4.0 %ASTM D1003
Gloss 95 %95 %20°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 150 - 175 °C302 - 347 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Elvax® 3165Z Ethylene Vinyl Acetate
DuPont Elvax® 3136 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
DuPont Elvax® 3135B Ethylene Vinyl Acetate
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film

PDUPH3 / 33606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.