MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the backup lining. It resists compression during operation which helps maintain lining stability. Applications Backup insulation for: - Continuous casting ladles
- Single-pour ladles
- Torpedo tube cars
- Tapping or transfer ladles
- Over the road crucibles
Advantages - Low thermal conductivity
- Reduces heat flow through ladle wall
- Longer working times for metal pouring or storage
- Minimal change in refractory layout
- Minimizes loss in ladle capacity
- Reduces shell temperature
- Not wet by molten aluminum
- Reduces installation times
- Increases lining stability
Information provided by Pyrotek. |