MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall MD-5009 Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf MD-5009 is a rigid, fitting-grade PVC compound designed for hot spruce/runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which includes color hold, regrind stability and surface appearance. MD-5009 is NSF listed under Standard 14/61 for both potable water and DWV applications.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D-955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 49.0 MPa7100 psiASTM D-638
Tensile Modulus 2.90 GPa420 ksiASTM D-638
Flexural Strength 89.6 MPa13000 psiASTM D-790
Flexural Modulus 2.96 GPa430 ksiASTM D-790
Izod Impact, Notched  0.374 J/cm
@Thickness 3.17 mm,
Temperature -20.0 °C
0.700 ft-lb/in
@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
 0.587 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.00 °C159.8 °FASTM D-648
Oxygen Index 38 %38 %ASTM D-2863
 
Descriptive Properties
Cell Classification, ASTM D-178412454NSF std. 14
Flow Ratio (Distance/Wall Thickness, 390-400°F)175Georgia Gulf Test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 8150 Rigid PVC, Extrusion & Molding
Axiall 1601 Clear 7002 Flexible PVC
Axiall 6511 Rigid PVC, Molding
Axiall 6316 Rigid PVC, Molding
Axiall 6300 Rigid PVC, Molding

PGGUL498 / 41774

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.