MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2099 X 121216 G Polylactic Acid (PLA) Impact Modified - 80% Bio-Content  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D 792
Linear Mold Shrinkage 0.0040 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0090 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 36.5 MPa5300 psiASTM D 638
Elongation at Break >= 5.0 %>= 5.0 %ASTM D 638
Tensile Modulus 2.21 GPa320 ksiASTM D 638
Flexural Strength 60.7 MPa8800 psiASTM D 790
Flexural Modulus 2.48 GPa360 ksiASTM D 790
Izod Impact, Notched 2.14 J/cm
@Thickness 3.20 mm
4.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 13.3 J/cm
@Thickness 3.20 mm
25.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 51.7 °C125 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 166 - 193 °C330 - 380 °F
Mold Temperature 15.6 - 29.4 °C60.0 - 85.0 °F
Drying Temperature 54.4 °C
@Time 7200 - 21600 sec
130 °F
@Time 2.00 - 6.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA)
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA)
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA)
NatureWorks® Ingeo™ 3251D Injection Grade PLA

PQZVA15391 / 120521

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.