MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Magnesium ZC63-T6
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes:

Key Words: UNS M16631; Mg
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.87 g/cc0.0676 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6060500 kg load, 10 mm ball
Hardness, Knoop 8080Estimated from Brinell
Hardness, Vickers 6868Estimated from Brinell
Tensile Strength, Ultimate 210 MPa30500 psi
Tensile Strength, Yield 125 MPa
@Strain 0.2 %
18100 psi
@Strain 0.2 %
Elongation at Break 4.0 %4.0 %in 50 mm
Tensile Modulus 45.0 GPa6530 ksi
Poissons Ratio 0.270.27
Shear Modulus 17.0 GPa2470 ksiEstimated from similar Mg alloys.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000540 ohm-cm0.00000540 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 370 J/g159 BTU/lbEstimated from trends in similar Mg alloys.
CTE, linear  26.0 µm/m-°C
@Temperature 0.000 - 100 °C
14.4 µin/in-°F
@Temperature 32.0 - 212 °F
Estimated from similar Mg alloys.
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
15.0 µin/in-°F
@Temperature 68.0 - 392 °F
Estimated from similar Mg alloys
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°FTypical Mg alloy value.
Thermal Conductivity 122 W/m-K847 BTU-in/hr-ft²-°F
Melting Point 465 - 635 °C869 - 1180 °F
Solidus 465 °C869 °F
Liquidus 635 °C1180 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 2.4 - 3.0 %2.4 - 3.0 %
Magnesium, Mg 91 %91 %As Remainder
Manganese, Mn 0.25 - 0.75 %0.25 - 0.75 %
Nickel, Ni <= 0.010 %<= 0.010 %
Silicon, Si <= 0.20 %<= 0.20 %
Zinc, Zn 5.5 - 6.5 %5.5 - 6.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium ZC71-T6
Magnesium ZC71, As-Extruded
Magnesium ZC71-T5
Magnesium ZC71-T6, Extruded Bars/Shapes
Magnesium ZE63A-T6, Cast

MMZC63 / 12466

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.