MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nickel silver 55-18, UNS C77000, H06 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Fabricated by blanking, forming and bending, and shearing.

Applications: optical goods, springs and resistance wire.

Test specimen: flat products - 1mm thickness.

Key Words: NS107, ISO CuNi18Zn27, CEN CW410J
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.70 g/cc0.314 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 96
@Thickness 1.00 mm
96
@Thickness 0.0394 in
Flat products
Hardness, Rockwell 30T 80
@Thickness 1.00 mm
80
@Thickness 0.0394 in
Flat products
Tensile Strength, Ultimate 745 MPa
@Thickness 1.00 mm
108000 psi
@Thickness 0.0394 in
Flat products
Tensile Strength, Yield 620 MPa
@Strain 0.5 %
89900 psi
@Strain 0.5 %
Flat products, 1 mm thick
Elongation at Break 2.5 %
@Thickness 1.00 mm
2.5 %
@Thickness 0.0394 in
in 50 mm, Flat products
Modulus of Elasticity 125 GPa18100 ksi
Poissons Ratio 0.330.33calculated
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 47.0 GPa6820 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000314 ohm-cm0.0000314 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.28 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 29.0 W/m-K
@Temperature 20.0 °C
201 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1055 °C<= 1931 °F
Liquidus 1055 °C1931 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 600 - 825 °C1110 - 1520 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 53.5 - 56.5 %53.5 - 56.5 %
Iron, Fe <= 0.25 %<= 0.25 %
Lead, Pb <= 0.10 %<= 0.10 %
Manganese, Mn <= 0.50 %<= 0.50 %
Nickel, Ni 16.5 - 19.5 %16.5 - 19.5 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 27 %27 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel silver 55-18, UNS C77000, H04 Temper flat products
Nickel silver 55-18, UNS C77000
Nickel silver 55-18, UNS C77000, H08 Temper flat products
Nickel silver 55-18, UNS C77000, OSO35 Temper flat products
Eagle Brass 770 Nickel Silver 18%, Spring

MC77000b4 / 11834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.