MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm0.011 - 0.014 in/in
Linear Mold Shrinkage, Transverse 0.0115 - 0.0145 cm/cm0.0115 - 0.0145 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 18.0 MPa
@Temperature 23.0 °C
2610 psi
@Temperature 73.4 °F
Elongation at Break  >= 100 %
@Temperature 23.0 °C
>= 100 %
@Temperature 73.4 °F
 >= 100 %
@Temperature 60.0 °C
>= 100 %
@Temperature 140 °F
 >= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
Elongation at Yield  6.0 %
@Temperature 23.0 °C
6.0 %
@Temperature 73.4 °F
 8.5 %
@Temperature 60.0 °C
8.5 %
@Temperature 140 °F
 9.0 %
@Temperature 90.0 °C
9.0 %
@Temperature 194 °F
Tensile Modulus  0.650 GPa
@Temperature 90.0 °C
94.3 ksi
@Temperature 194 °F
 1.10 GPa
@Temperature 60.0 °C
160 ksi
@Temperature 140 °F
 2.60 GPa
@Temperature 23.0 °C
377 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched  1.50 J/cm²
@Temperature -20.0 °C
7.14 ft-lb/in²
@Temperature -4.00 °F
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.100 J/cm²
@Temperature -20.0 °C
0.476 ft-lb/in²
@Temperature -4.00 °F
 0.350 J/cm²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °F
Vicat Softening Point 95.0 °C
@Load 5.00 kg
203 °F
@Load 11.0 lb
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
Oxygen Index 24 %24 %
Glow Wire Test  750 °C
@Thickness 1.00 mm
1380 °F
@Thickness 0.0394 in
GWFI/GWT
 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 240 °C392 - 464 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
176 - 194 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Borealis Bormed™ BE860MO Polypropylene Copolymer for Healthcare Applications
Flint Hills 44S2A Polypropylene Impact Copolymer

PLATH9830 / 177526

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.