MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® B 230 Grey 1429 H PA 66/6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: TECHNYL® B 230 Grey 1429 H is an unfilled copolyamide 6.6/6, impact modified, for injection molding. The product is available in grey color.

Key Properties: Medium impact; High flexibility; Good surface aspect

Benefits: This product offers an excellent notched impact resistance, even at low temperature.

Applications: The product is suitable for sport and leisure applications, such as for shoe soles, ski components, ski or surf bindings.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183/A
Water Absorption 1.35 %
@Time 86400 sec
1.35 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0107 cm/cm0.0107 in/inIsotropy
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/in
Linear Mold Shrinkage, Transverse 0.0205 cm/cm0.0205 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiISO 527 Type 1A
Tensile Strength, Yield 45.0 MPa6530 psiISO 527 Type 1A
Elongation at Break 250 %250 %ISO 527 Type 1A
Elongation at Yield 12 %12 %ISO 527 Type 1A
Tensile Modulus 0.900 GPa131 ksiISO 527 Type 1A
Flexural Strength 27.0 MPa3920 psiISO 178
Flexural Modulus 0.700 GPa102 ksiISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²8.57 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 16.0 kV/mm406 kV/inIEC 60243
Dissipation Factor 0.0700.070IEC 60250
Comparative Tracking Index 600 V600 VSol A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 242 °C468 °FISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® GP52DB Ester Based Thermoplastic Polyurethane
Domo TECHNYL® A 258P1 Black 2N PA 66, Dry
Domo TECHNYL® B 230 Black-H PA 66/6, Conditioned
Markforged Nylon 3D Printed Polymer
DSM Fibre Intermediates Nyrim® 3000 (Dry)

PSOLVAY852 / 218580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.