MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properties than many unreinforced thermoplastic polyester and nylon resins especially after exposure to humid environments.

These materials were specifically designed for automotive electrical and electronic applications such as connectors, sockets, and sensors. Additional applications include fuel systems where both the high elongation/ductility and superior low permeation performance to automotive fuels are needed.

They can be processed readily using conventional injection molding equipment and methods.

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Moisture Absorption at Equilibrium 0.50 %0.50 %24 hours; ASTM D570
Linear Mold Shrinkage 0.019 cm/cm0.019 in/in93°C; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.0 MPa7400 psiASTM D638
Elongation at Yield 50 %50 %ASTM D638
Tensile Modulus 2.50 GPa363 ksiASTM D638
Flexural Strength 71.0 MPa10300 psiASTM D790
Flexural Modulus 1.90 GPa276 ksiASTM D790
Shear Strength 47.0 MPa6820 psiASTM D732
Izod Impact, Notched 8.00 J/cm15.0 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Dynatup @ -18°C 47.0 J34.7 ft-lbTotal Energy. 50% RH. No temperature indicated.; D3763
Dynatup @ -18°C Max Load 408000 g900 lbNo temperature indicated.; D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.50e+15 ohm-cm2.50e+15 ohm-cmASTM D257
Surface Resistance 2.50e+15 ohm2.50e+15 ohmASTM D257
Dielectric Constant  3.6
@Frequency 60 Hz
3.6
@Frequency 60 Hz
ASTM D150
 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor  0.012
@Frequency 60 Hz
0.012
@Frequency 60 Hz
ASTM D150
 0.027
@Frequency 1e+6 Hz
0.027
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V>= 600 VASTM D3638
High Voltage Arc-Tracking Rate, HVTR 8.80 mm/min0.346 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 300 °C572 °FASTM D3418
Shrinkage 2.0 %2.0 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 L Polyphthalamide (PPA) Resin, at 50% RH
RTP Company RTP 4000 ET-1001 L Polyphthalamide (PPA), Impact Modified - Lubricated
DuPont Mobility and Materials Zytel® HTN FE350038 BK083 Polyphthalamide (PPA)

PSOLVT89 / 21385

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.