MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D1163 P (SIS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1163 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:
Kraton D1163 PT - supplied as a dusted dense pellet
Kraton D1163 PTM - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1163 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen Modification

Note 1) The final dusting level is a combination of the talc from the original D1163PT plus silica added during the milling process.

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D4025
Volatiles <= 0.50 %<= 0.50 %KM 04
Viscosity 900 cP900 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 23 g/10 min
@Load 5.00 kg,
Temperature 200 °C
23 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Ash 0.25 - 0.45 %0.25 - 0.45 %PT, Talc; BAM 908
 2.5 - 5.0 %2.5 - 5.0 %PTM, See note 1); ISO 247
 
Chemical PropertiesMetricEnglishComments
Diblock Content 38 %38 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 25
@Time 10.0 sec
25
@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 10.34 MPa1500 psiTypical properties of film cast from toluene solution; ASTM D412
Elongation at Break 1400 %1400 %Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.430 MPa
@Strain 300 %
62.4 psi
@Strain 300 %
film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentAntioxidant0.08-0.3%, KM 08
 Polystyrene13.3-16.3%, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber Ratio15/85

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1114 P (SIS) Linear Triblock Copolymer
Kraton® D1161 P (SIS) Linear Triblock Copolymer
Kraton® D1117 P (SIS) Linear Triblock Copolymer
Kraton® D1113 P (SIS) Linear Block Copolymer
Kraton® D1119 P (SIS) Linear Triblock Copolymer

PKRA9872 / 132771

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.