MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Filler Content 40 %40 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm
@Thickness 3.18 mm
0.020 - 0.040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 221 MPa32100 psi5.1 mm/min; ASTM D638
Elongation at Break 1.0 %1.0 %5.1 mm/min; ASTM D638
Tensile Modulus 37.9 GPa5500 ksi5.1 mm/min; ASTM D638
Flexural Strength 331 MPa48000 psi1.3 mm/min; ASTM D790
Flexural Modulus 26.2 GPa3800 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.680 J/cm1.27 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 10000 ohm-cm100 - 10000 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
@Thickness 3.18 mm
473 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Descriptive Properties
FeaturesFlame Retardant
 High Stiffness
 Semi Crystalline
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAerospace Applications
 Automotive Electronics
 Business Equipment
 Computer Components
 Connectors
 Consumer Applications
 Electrical Housing
 Electrical/Electronic Applications
 Structural Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA E830iPd LCP, 30% Specialty
Avient Edgetek® NN-20CF/000 BLACK Polyamide 66 (Nylon 66)
Avient Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66)
Avient Edgetek® NN-40CF/000 Nylon 6/6, Carbon Fiber Reinforced
Avient Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66)

PH0POL1070 / 145639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.