  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Indium Corp. Indalloy 39 Bismuth Solder Alloy
Categories: Metal; Nonferrous Metal; Bismuth Alloy; Solder/Braze Alloy

Material Notes: Low temperature eutectic solder paste. Can be used on the same metallization as SnPb based solders.

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.60 g/cc0.347 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 15.5
@Load 4.00 kg
15.5
@Load 8.82 lb
2mm ball
Tensile Strength at Break 35.9 MPa5200 psi
Elongation at Break 100 %100 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000750 ohm-cm0.0000750 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 34.7 J/g14.9 BTU/lb
Specific Heat Capacity 0.151 J/g-°C0.0361 BTU/lb-°FSolid
 0.167 J/g-°C0.0399 BTU/lb-°FLiquid
Thermal Conductivity 13.0 W/m-K
@Temperature 85.0 °C
90.2 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 96.0 °C205 °FEutectic
Solidus 96.0 °C205 °F
Liquidus 96.0 °C205 °F
 
Component Elements PropertiesMetricEnglishComments
Bismuth, Bi 52 %52 %
Lead, Pb 30 %30 %
Tin, Sn 18 %18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AIM 47 Fusible Bismuth Alloy
Indium Corp. Indalloy® 158 Bi-Pb-Sn-Cd Solder Alloy
AIM 58 Fusible Alloy
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging
AIM 70 Fusible Alloy

NNIN729 / 97938

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.