MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem PB208 Injection Molding Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Injected lids and caps; Large flat surface injected pieces.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.923 g/cc0.923 g/ccASTM D1505/D792
ESCR 10% Igepal® 3.0 hour
@Temperature 50.0 °C
3.0 hour
@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
22 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4242ASTM D2240
Tensile Strength at Break 6.00 MPa870 psiASTM D638
Tensile Strength, Yield 10.0 MPa1450 psiASTM D638
Flexural Modulus, 1% Secant 700 MPa102000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 87.0 °C189 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem PB608 Injection Molding Low Density Polyethylene
SCG Chemicals EL-Lene™ D682PC Low Density Polyethylene Pipe Resin
Dow LDPE 779I Low Density Polyethylene
Dow LDPE 722M Low Density Polyethylene
Breplast Bretene LD PIPE Low Density Polyethylene

PBRAS755 / 109530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.