MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Covestro Makrolon® Rx1452 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: MVR (300 °C/1.2 kg) 16 cm³/10 min; medical devices; low viscosity; easy release; injection molding - melt temperature 280 - 320 °C

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.660 g/cc0.0238 lb/in³pellets; IOS 60
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.12 %0.12 %ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inparallel/normal; b.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in60x60x2 mm; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in60x60x2 mm; 280 °C / MT 80 °C; 500 bar; ISO 294-4
Melt Flow 17 g/10 min
@Load 1.20 kg,
Temperature 300 °C
17 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1/-2
 130 %130 %50 mm/min; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 100 MPa14500 psi2 mm/min; ISO 178
Flexural Yield Strength 78.0 MPa
@Strain 3.2 %
11300 psi
@Strain 3.2 %
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2 mm/min; ISO 178
Flexural Strain at Yield 6.8 %6.8 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
5.71 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 180-A
 65.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
30.9 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Impact 53005300Puncture - maximum force (N); ISO 6603-2
 6200
@Temperature -30.0 °C
6200
@Temperature -22.0 °F
Puncture - maximum force (N); ISO 6603-2
Puncture Energy 60.0 J44.3 ft-lbISO 6603-2
 65.0 J
@Temperature -30.0 °C
47.9 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°Fcross-flow; ISO 8302
Hot Ball Pressure Test 118 °C244 °FISO 2039-1
 132 °C270 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FISO 75-1/-2
Vicat Softening Point 140 °C284 °F50°C/h 50N; ISO 306
 141 °C286 °F120°C/h 50N; ISO 306
Flash Point 480 °C896 °Fignition; ASTM D1929
 550 °C1020 °Fself ignition; ASTM D1929
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %
@Thickness 76.2 mm
1.0 %
@Thickness 3.00 in
ISO 14782
Transmission, Visible 86 %
@Thickness 76.2 mm
86 %
@Thickness 3.00 in
ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection Molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® M90™ POM, Unfilled
INEOS Styrolution Terlux® HD 2812 MABS
LyondellBasell Alathon® M5370 High Density Polyethylene
Covestro Makrolon® 2405 MAS048 Polycarbonate
Covestro Makrolon® 3156 Polycarbonate

PB09967 / 92807

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.