MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 304 Cast Stainless Steel, ASTM A276 Cold Formed
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic

Key Words: ASTM A 276-000
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  >= 515 MPa
@Thickness >=12.7 mm
>= 74700 psi
@Thickness >=0.500 in
 >= 620 MPa
@Thickness <=12.7 mm
>= 89900 psi
@Thickness <=0.500 in
Tensile Strength, Yield  >= 205 MPa
@Thickness >=12.7 mm
>= 29700 psi
@Thickness >=0.500 in
 >= 310 MPa
@Thickness <=12.7 mm
>= 45000 psi
@Thickness <=0.500 in
Elongation at Break  >= 30 %
@Thickness <=12.7 mm
>= 30 %
@Thickness <=0.500 in
 >= 30 %
@Thickness >=12.7 mm
>= 30 %
@Thickness >=0.500 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe >= 66 %>= 66 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 11 %8.0 - 11 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 304 Cast Stainless Steel, ASTM A276 Hot Formed
AISI 304 Cast Stainless Steel, UNS J92610
AISI 304 Cast Stainless Steel, EN 10088-3
AISI 304 Cast Stainless Steel, SUS304
304 Stainless Steel

MQCS304C / 157357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.