MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Delrin Delrin® SC655 NC010 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Water Absorption 1.4 %
@Thickness 2.00 mm
1.4 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.300 %
@Thickness 2.00 mm
0.300 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4, 2577
Melt Flow 15 g/10 min15 g/10 minISO 1133
 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
13 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 2000 N
@Temperature 23.0 °C
450 lb (f)
@Temperature 73.4 °F
maximum force; ISO 6603-2
Hardness, Rockwell M 9292ISO 2039-2
Hardness, Rockwell R 120120ISO 2039-2
Tensile Strength, Yield 71.0 MPa10300 psiISO 527-1/-2
Elongation at Break 30 %30 %Nominal; ISO 527-1/-2
Elongation at Yield 17 %17 %ISO 527-1/-2
Tensile Modulus 3.10 GPa450 ksiISO 527-1/-2
Flexural Strength 80.0 MPa
@Strain 3.5 %
11600 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.95 GPa428 ksiISO 178
Poissons Ratio 0.370.37
Izod Impact, Notched (ISO)  8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 9.00 kJ/m²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  250 kJ/m²
@Temperature -30.0 °C
119 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1U
 280 kJ/m²
@Temperature 23.0 °C
133 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  28.0 J/cm²
@Temperature -30.0 °C
133 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 30.0 J/cm²
@Temperature 23.0 °C
143 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Puncture Energy 3.00 J
@Temperature 23.0 °C
2.21 ft-lb
@Temperature 73.4 °F
ISO 6603-2
Tensile Creep Modulus, 1 hour 2800 MPa406000 psi1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 1600 MPa232000 psi1000h; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmIEC 62631-3-1
Surface Resistance 4.00e+14 ohm4.00e+14 ohmIEC 62631-3-2
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 44.0 kV/mm1120 kV/inIEC 60243-1
Dissipation Factor  0.0055
@Frequency 1e+6 Hz
0.0055
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.0090
@Frequency 100 Hz
0.0090
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Hot Ball Pressure Test 165 °C329 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1/-2
Vicat Softening Point 155 °C311 °F50°C/h, 50N; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 215 °C419 °FOptimum, Injection
 210 - 220 °C410 - 428 °FRange, Injection
Mold Temperature 90.0 °C194 °FOptimum, Injection
 80.0 - 100 °C176 - 212 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %<= 0.20 %Injection
Hold Pressure 80.0 - 100 MPa11600 - 14500 psiInjection
 100 MPa14500 psiInjection
Annealing Temperature 160 °C320 °FOptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Emissions (mg/kg)<8VDA 275
Fogging (%)90F-value (refraction); ISO 6452
Fogging (mg)0.35G-value (condensate); ISO 6452
Part Marking Code>POM<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)8Injection
Resin IdentificationPOMISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Delrin® SC699 NC010 POM
INEOS Styrolution Novodur® M203FC ABS
Colorite Polymers 1124 Clear Injection Molding Vinyl Compound
INEOS Styrolution Terlux® 2802 Transparent MABS
Delrin Delrin® 500CL BK601 POM

PDSX5163 / 197803

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.