BETAFOAM™ 87100/87120 is a low density, all water blown rigid polyurethane foam. These components were engineered to produce a foam for providing barrier protection against airborne noise. Foam is produced by the rapid mixing of both components under high shear conditions. These components were formulated for fast reaction and high volume expansion. The foam has adhesion to primed metal surfaces. Information provided by Dow |