MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Petromont 3000 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and other similar objects requiring rigidity, toughness and freedom from warpage.

Petromont HDPE 3000 is a medium molecular weight homopolymer resin. Its very narrow molecular weight distribution and high density make it ideally suited for injection moulding applications where outstanding stiffness, warp resistance and toughness are demanded. Parts moulded from Petromont HDPE 3000 exhibit high gloss, low odour and are suitable for food packaging applications.

Key Words: Food grade, crates, cases, trays
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.965 g/cc0.0349 lb/in³ASTM D1505
ESCR 10% Igepal® 40 hour40 hourF50; ASTM D1693
Melt Flow 8.9 g/10 min8.9 g/10 minI2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.4 MPa4700 psiASTM D638
Flexural Modulus 1.72 GPa249 ksiASTM D790
Tensile Impact Strength 67.3 kJ/m²32.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -100 °C<= -148 °FASTM D746
 
Descriptive Properties
ProcessInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 3252 Polyethylene, Injection Grade
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding
Aclo Accucomp Polyethylene HD0200L High Density
Braskem IA59 HDPE Injection Molding Polyethylene Homopolymer

PPETROM11 / 56205

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.