MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Anhydride-Modified Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Anhydride-Modified Polyethylene

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 - 0.960 g/cc0.0314 - 0.0347 lb/in³Average value: 0.921 g/cc Grade Count:87
Particle Size 125 - 500 µm125 - 500 µmAverage value: 283 µm Grade Count:3
Water Vapor Transmission 4.30 - 17.8 g/m²/day0.277 - 1.15 g/100 in²/dayAverage value: 7.51 g/m²/day Grade Count:12
Viscosity 600 - 4200 cP
@Temperature 140 - 140 °C
600 - 4200 cP
@Temperature 284 - 284 °F
Average value: 1.60e+6 cP Grade Count:6
 900000 - 3.00e+6 cP
@Temperature 190 - 190 °C
900000 - 3.00e+6 cP
@Temperature 374 - 374 °F
Average value: 1.60e+6 cP Grade Count:15
 900000 - 3.00e+6 cP
@Shear Rate 50.0 - 50.0 1/s
900000 - 3.00e+6 cP
@Shear Rate 50.0 - 50.0 1/s
Average value: 1.60e+6 cP Grade Count:15
Oxidative Induction Time (OIT) 10.0 - 123 min10.0 - 123 minAverage value: 80.2 min Grade Count:7
 20.0 - 20.0 min
@Temperature 210 - 210 °C
20.0 - 20.0 min
@Temperature 410 - 410 °F
Average value: 20.0 min Grade Count:2
Methyl Acrylate Content 20.0 - 24.0 %20.0 - 24.0 %Average value: 21.3 % Grade Count:3
Thickness 50.8 microns2.00 milAverage value: 50.8 microns Grade Count:11
Melt Flow 0.400 - 31.0 g/10 min0.400 - 31.0 g/10 minAverage value: 3.76 g/10 min Grade Count:87
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 30.0 - 65.030.0 - 65.0Average value: 47.6 Grade Count:12
Tensile Strength, Ultimate 6.00 - 30.0 MPa870 - 4350 psiAverage value: 16.6 MPa Grade Count:8
Film Tensile Strength at Yield, MD 5.50 - 21.7 MPa798 - 3150 psiAverage value: 11.4 MPa Grade Count:12
Film Tensile Strength at Yield, TD 5.70 - 23.2 MPa827 - 3360 psiAverage value: 12.6 MPa Grade Count:12
Tensile Strength, Yield 4.50 - 25.0 MPa653 - 3630 psiAverage value: 15.2 MPa Grade Count:13
Film Elongation at Break, MD 450 - 890 %450 - 890 %Average value: 687 % Grade Count:12
Film Elongation at Break, TD 290 - 920 %290 - 920 %Average value: 704 % Grade Count:12
Film Elongation at Yield, MD 4.00 - 30.0 %4.00 - 30.0 %Average value: 15.2 % Grade Count:12
Film Elongation at Yield, TD 2.00 - 22.0 %2.00 - 22.0 %Average value: 10.0 % Grade Count:12
Elongation at Break 90.0 - 930 %90.0 - 930 %Average value: 548 % Grade Count:17
Modulus of Elasticity 0.400 - 1.07 GPa58.0 - 155 ksiAverage value: 0.888 GPa Grade Count:4
Flexural Modulus 0.0220 - 0.758 GPa3.19 - 110 ksiAverage value: 0.385 GPa Grade Count:3
Peel Strength >= 40.0 kN/m
@Temperature 80.0 - 80.0 °C
>= 228 pli
@Temperature 176 - 176 °F
Average value: 40.0 kN/m Grade Count:1
Elmendorf Tear Strength MD 28.0 - 640 g28.0 - 640 gAverage value: 240 g Grade Count:12
Elmendorf Tear Strength TD 39.0 - 1100 g39.0 - 1100 gAverage value: 503 g Grade Count:12
Elmendorf Tear Strength, MD 0.551 - 12.6 g/micron14.0 - 320 g/milAverage value: 6.83 g/micron Grade Count:4
Elmendorf Tear Strength, TD 0.768 - 21.7 g/micron19.5 - 550 g/milAverage value: 13.7 g/micron Grade Count:4
Film Tensile Strength at Break, MD 8.10 - 52.1 MPa1170 - 7560 psiAverage value: 27.6 MPa Grade Count:12
Film Tensile Strength at Break, TD 2.10 - 40.0 MPa305 - 5800 psiAverage value: 22.2 MPa Grade Count:12
 
Thermal PropertiesMetricEnglishComments
Melting Point 53.9 - 160 °C129 - 320 °FAverage value: 114 °C Grade Count:57
Crystallization Temperature 43.0 - 144 °C109 - 291 °FAverage value: 96.6 °C Grade Count:7
Deflection Temperature at 0.46 MPa (66 psi) 58.0 - 73.0 °C136 - 163 °FAverage value: 68.0 °C Grade Count:3
Vicat Softening Point 40.0 - 129 °C104 - 264 °FAverage value: 92.0 °C Grade Count:61
Glass Transition Temp, Tg -56.0 - -49.0 °C-68.8 - -56.2 °FAverage value: -53.0 °C Grade Count:3
Dropping Point 106 - 116 °C223 - 241 °FAverage value: 109 °C Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 270 °C320 - 518 °FAverage value: 234 °C Grade Count:21
Nozzle Temperature 235 °C455 °FAverage value: 235 °C Grade Count:16
Adapter Temperature 230 °C446 °FAverage value: 230 °C Grade Count:4
Die Temperature 220 - 250 °C428 - 482 °FAverage value: 238 °C Grade Count:6
Melt Temperature 160 - 240 °C320 - 464 °FAverage value: 206 °C Grade Count:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
LyondellBasell Lucalen A2920M Low Density Polyethylene
Overview of materials for Low Density Polyethylene (LDPE), Molded
Celanese 191A LDPE polymer for adhesives, automotive and compounds
ExxonMobil EXACT™ 4150 Plastomer

O4090 / 78290

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.