MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

CPT C-Flex® R70-116 Opaque Biocompatible TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current United States Pharmacopoeia Class VI test requirements. C-Flex® does not contain latex rubber, polyvinyl chloride, silicone rubber, or polyurethane.

Information provided by Consolidated Polymer Technologies.

Key Words: SEBS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D 792
Linear Mold Shrinkage 0.018 - 0.020 cm/cm0.018 - 0.020 in/in
Melt Flow 2.4 g/10 min2.4 g/10 minCondition E; ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30301 sec.; ASTM D 2240
Tensile Strength at Break 7.619 MPa1105 psiASTM D 412
Elongation at Break 810 %810 %ASTM D 412
100% Modulus 0.689 MPa
@Strain 100 %
100 psi
@Strain 100 %
ASTM D 412
300% Modulus 1.03 MPa
@Strain 300 %
150 psi
@Strain 300 %
ASTM D 412
Tear Strength 14.7 kN/m84.0 pliNotched, Die B; ASTM D 624
 21.7 kN/m124 pliDie C; ASTM D 624
Taber Abrasion, mg/1000 Cycles 581581Federal Test Method Standard, 405
Compression Set  24 %
@Temperature 23.0 °C
24 %
@Temperature 73.4 °F
ASTM D 412
 86 %
@Temperature 70.0 °C
86 %
@Temperature 158 °F
ASTM D 412
Tensile Set 6.0 %6.0 %at 300% elongation; ASTM D 412
 17 %17 %at break; ASTM D 412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 163 - 204 °C325 - 400 °FExtrusion Temperature
Middle Barrel Temperature 149 - 218 °C300 - 425 °FInjection molding cylinder temperature
Drying Temperature 65.6 - 93.3 °C150 - 200 °FDesiccant type
Injection Pressure 2.07 - 6.89 MPa300 - 1000 psi
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Sterilization methods:Cobalt 60, Ethylene OxideSteam/Autoclave not recommended

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CPT C-Flex® R70-214 Opaque Biocompatible TPE
CPT C-Flex® R70-026 Opaque Biocompatible TPE
CPT C-Flex® R70-051 Clear Biocompatible TPE
CPT C-Flex® R70-190 Opaque Biocompatible TPE
CPT C-Flex® R70-028 Opaque Biocompatible TPE

PCPT02 / 29097

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.