MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals Udimet® 500 Nickel Alloy (UNS N07500)  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Precipitation Hardening Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.02 g/cc0.290 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  221 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
32000 psi
@Temperature 1500 °F,
Time 1000 hour
 324 MPa
@Temperature 816 °C,
Time 360000 sec
47000 psi
@Temperature 1500 °F,
Time 100 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.3 µm/m-°C
@Temperature 20.0 - 100 °C
6.28 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 11.3 W/m-K
@Temperature 20.0 - 100 °C
78.3 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.0 %3.0 %
Boron, B 0.005 %0.005 %
Carbon, C 0.08 %0.08 %
Chromium, Cr 19 %19 %
Cobalt, Co 19 %19 %
Iron, Fe <= 4.0 %<= 4.0 %
Molybdenum, Mo 4.0 %4.0 %
Nickel, Ni 48 %48 %
Titanium, Ti 3.0 %3.0 %

References for this datasheet.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals Udimet® 700 Nickel Alloy
Special Metals UDIMET® alloy 720 Nickel Base Alloy
Special Metals Udimet® 630 Nickel Alloy Composition Spec
Special Metals UDIMET® alloy 520 Superalloy
Special Metals INCONEL® Alloy 718

NINDA17s / 150727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.