MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay FT8 Adhesive tape
Categories: Polymer; Adhesive; Tape

Material Notes: Description: Adhesive tape. Ideally suited to metal bonding applications.

Features & Benefits:

  • Polyester tape backed with a fully cured, pressure sensitive adhesive.
  • Excellent temperature resistance
  • Strips easily after use.
  • Ideal for use when silicone adhesives are likely to cause surface contamination, such as in metal bonding applications.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.0 microns1.97 milAdhesive
 50.0 microns1.97 milTape
 100 microns3.94 milTotal
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GrafTech P6A6 Ultra-Thin, Double-Coated Adhesive Tape
GrafTech P1A1 Double-Coated Adhesive Tape
Solvay Flashtape 5H Adhesive tape
Solvay 6325-05 Adhesive tape
Saint-Gobain Chemlam® SGC6-10 Copper Adhesive Tape

PCYTED230 / 180532

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.