MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hong Kun Group HBCD Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical name: Hexabromocyclododecane. HBCD flame retardant is used primarily in extruded (XPS) or suspension-polymerized polystyrene foam (EPS). With a stabilization package and proper processing conditions, it can be used in polystyrene and polypropylene resins. It can also be used in textile treatments, adhesives and coating applications.

CAS No. 3194-55-6

All information provided by Hongkun Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Evaporation Loss <= 0.50 %<= 0.50 %loss on drying
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 178 °C>= 352 °F
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br >= 74.0 %>= 74.0 %
 
Descriptive Properties
Appearancewhite powder
Color, APHA>= 20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc Fluoroborate Hexahydrate, Zn(BF4)2-6H2O
Solvay RHODAFAC® RS-610/A25 Surfactant
Oceanchem Group 1,2,5,6,9,10-Hexabromocyclododecane (HBCD)
LG Chemical R320 EPS, Flame Retardant
LG Chemical R240 EPS, Flame Retardant

PHONGK022 / 86323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.