MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP

Material Notes: SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ASTM D2240
Tensile Strength, Ultimate 49.0 MPa7110 psiASTM D638
Tensile Stress at Strain  6.37 MPa
@Strain 5.0 %
925 psi
@Strain 5.0 %
ASTM D638
 10.8 MPa
@Strain 10 %
1560 psi
@Strain 10 %
ASTM D638
Elongation at Break 900 %900 %ASTM D638
Flexural Modulus 0.206 GPa29.9 ksiASTM D790
Tear Strength 165 kN/m941 pliASTM D1004
 
Thermal PropertiesMetricEnglishComments
Melting Point 205 °C401 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals SKYPEL G155D General Grade
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion
Samyang Triel® 5450 Thermoplastics Polyetherester Elastomer, General Extrusion
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer

PSK119 / 67851

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.