MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for high temperature applications. The nitrogen additions stabilize the austenitic microstructure, particularly at high temperatures. The alloy is less susceptible to embrittlement effects occurring after long term exposure. Creep properties are enhanced, due to high Chromium and Nitrogen. Rare Earth elements (Ce, La,...) are added in order to anchor the oxide protective film and improve the resistance of the steel to oxide spalling. As a result, the alloy is much more resistant to high temperature thermal cycling effects in oxidizing atmospheres compared to 310. CLI SIRIUS S15 grade may be used up to 1100°C (2012°F in oxidizing environments. Thermal cycling effects, sulphur containing atmospheres and low oxygen contents reduce the high temperature resistance of the steel.

>Information provided by manufacturer.

Key Words: EN 10095 X9 Cr Ni Si N Ce 21-11-2 -1.4835, AFNOR (Z10 CNS 21 11), DIN W.Nr 1.4835, UNS S30815
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 680 MPa98600 psiTypical after Solution Annealing
Tensile Strength, Yield  350 MPa
@Strain 0.2 %
50800 psi
@Strain 0.2 %
Typical after Solution Annealing
 370 MPa
@Strain 1 %
53700 psi
@Strain 1 %
Typical after Solution Annealing
Elongation at Break 40 %40 %Typical
Creep Strength 200 MPa
@Temperature 600 °C,
Time 3.60e+6 sec
29000 psi
@Temperature 1110 °F,
Time 1000 hour
1% Creep Strain
Modulus of Elasticity 200 GPa29000 ksi
Poissons Ratio 0.3330.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
10900 ksi
@Temperature 68.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000900 ohm-cm
@Temperature 20.0 °C
0.0000900 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.89 µin/in-°F
@Temperature 68.0 - 212 °F
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
10.0 µin/in-°F
@Temperature 68.0 - 752 °F
 18.5 µm/m-°C
@Temperature 20.0 - 600 °C
10.3 µin/in-°F
@Temperature 68.0 - 1110 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
0.120 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.080 %0.080 %
Chromium, Cr 21 %21 %
Iron, Fe 66.01 %66.01 %As remainder
Nickel, Ni 11 %11 %
Nitrogen, N 0.17 %0.17 %
Rare Earths 0.040 %0.040 %
Silicon, Si 1.7 %1.7 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Crucible Steel SUE52 Martensitic Steel
Aluminum 5052-O
Aluminum 5052-H38
Aluminum 5052-H36

NINDUST28 / 17566

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.