MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt AL 716 Aluminum Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Solder/Braze Alloy

Material Notes: Applications:AL 716 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought should be given to the galvanic potential between the metals to avoid corrosion problems. The corrosion resistance of AL 716 is good. To maintain joint integrity on heat treatable aluminums, the solution temperature must be below the solidus of the filler metal.

Characteristics:AL 716 is a general purpose brazing filler metal for use with brazeable aluminums in all types of brazing processes. To prevent liquation, it is recommended that the parts be heated rapidly through the solidus-liquidus temperature range.

Specifications:AL 716 meets the requirements for the following specifications-Aluminum Association (AA) 4145, American Welding Society (AWS) A5.8 BAISi-3

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.71 g/cc0.0979 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 521 - 585.0 °C970 - 1085 °F
Solidus 521 °C970 °FMelting Point
Liquidus 585.0 °C1085 °FFlow Point
 
Processing PropertiesMetricEnglishComments
Processing Temperature 571 - 604 °C1060 - 1120 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 83 %>= 83 %
Chromium, Cr <= 0.15 %<= 0.15 %
Copper, Cu 3.3 - 4.7 %3.3 - 4.7 %
Iron, Fe <= 0.80 %<= 0.80 %
Magnesium, Mg <= 0.15 %<= 0.15 %
Manganese, Mn <= 0.15 %<= 0.15 %
Other, each <= 0.050 %<= 0.050 %
Other, total 0.15 %0.15 %
Silicon, Si 9.3 - 10.7 %9.3 - 10.7 %
Zinc, Zn <= 0.20 %<= 0.20 %
 
Descriptive Properties
ColorGrayish-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
4147 Aluminum Composition Spec
Aluminum 4045
AMG Aluminum Boral® 10% Boron Aluminum Alloy
AMG Aluminum Tibor® 1.7% Ti - 1.4% B Titanium Boron Aluminum Alloy

NLUCMI00 / 18067

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.