MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Henkel Bonderite 37 Make Up and Replenisher B Phosphate Conversion Coating
Categories: Fluid; Solvent

Material Notes: Bonderite 37 chemicals are formulated primarily for treating hot-dip galvanized and certain continuous electrogalvanized surfaces which are difficult to coat with other materials. Applied by spray or immersion, the treatment will prevent white spots, seediness and pinpoint buildup. Steel may be given an excellent coating by adding Accelerator 130 or 131, and the process is well suited for mixed production of galvanized and steel. Limited quantities of aluminum can be coated satisfactorily. If much aluminum is to be treated, other processes are preferred. Cadmium must never be run through the solution because it will poison the bath.

Application: Zinc Phosphate Conversion Coating

Key Words: Aerospace Surface Treatment
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
ChemistryZinc phosphate
ConsistencyLiquid
FormConcentrated
SubstrateFerrous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Bonderite 7400 Conversion Coating
Henkel Alodine T 5923 Conversion Coating
Henkel Alodine 5700 Wipes Conversion Coating, Touch Up
Henkel Bonderite 880 Make Up and Replenisher Phosphate Conversion Coating
Henkel Alodine T 5900 RTU Conversion Coating

PHENK912 / 146917

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.