MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovation Polymers Opnyl LSE - OP66GF3015 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Low surface energy Nylon 66 for demanding applications such as bearings, bushes, rods and gears

All properties after 48hrs conditioning at 23°C/50% RH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 135 MPa19600 psi50 mm/min; ASTM D638
Elongation at Break 3.8 %3.8 %50 mm/min; ASTM D638
Tensile Modulus 7.525 GPa1091 ksi50 mm/min; ASTM D638
Flexural Strength 195 MPa28300 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 6.895 GPa1000 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.908 J/cm1.70 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 242 °C
@Thickness 3.20 mm
468 °F
@Thickness 0.126 in
Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66
Ovation Polymers Nima™ NH PC143P Polycarbonate
Ovation Polymers Opnyl OP66GF43 Nylon 66, As Conditioned
Ovation Polymers Opnyl OP66GF43 Nylon 66, Dry as Molded
Ovation Polymers Opnyl OP66GF50 Nylon 66

POVAT144 / 79123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.