MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Aramid; Phenolic

Material Notes: Designation: Material-Cell Size-Density.
Hexweb® HRH-10 is manufactured from NOMEX® aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagonal or OX-Core® configuration, the block is dipped in phenolic resin. After curing the resin, slices are cut to the desired thickness. For special applications, such as air directionalizing, HexWeb® HRH-10 can be provided without the phenolic resin. Using this process, a wide range of cell sizes, paper thicknesses, and densities can be produced.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0288 g/cc0.00104 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength >= 0.655 MPa>= 95.0 psiBare, min
 >= 0.724 MPa>= 105 psiStabilized, min
 0.827 MPa120 psiBare, typical
 0.896 MPa130 psiStabilized, typical
Compressive Modulus 0.0552 GPa8.00 ksiStabilized, typical
Shear Modulus 0.0131 GPa1.90 ksiPlate Shear, W Direction, typical
 0.0262 GPa3.80 ksiPlate Shear, L Direction, typical
Shear Strength >= 0.276 MPa>= 40.0 psiPlate Shear, W Direction, min
 0.345 MPa50.0 psiPlate Shear, W Direction, typical
 >= 0.517 MPa>= 75.0 psiPlate Shear, L Direction, min
 0.621 MPa90.0 psiPlate Shear, L Direction, typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-10 - 1/4 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Hexcel® HexWeb® HRH-10 - 3/16 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb

PHEXC331 / 98802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.