RheTech Products P250-01 Polypropylene Copolymer, Black
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
Material Notes:
Applications:
Consoles
Consumer goods
Injection molding conditions reported in table.
Information provided by RheTech Products.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.910
g/cc
@Temperature 23.0 °C
0.910
g/cc
@Temperature 73.4 °F
23/23°C; ASTM D792
Linear Mold Shrinkage
0.0145
cm/cm
0.0145
in/in
ASTM D955
Melt Flow
8.0
g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
66
66
ASTM D2240
Tensile Strength at Break
26.5
MPa
3850
psi
2 in/min; ASTM D638
Flexural Modulus
1.17
GPa
170
ksi
Tangent; ASTM D790
Izod Impact, Notched
1.07
J/cm
@Temperature 23.0 °C
2.00
ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact
22.6
J
16.7
ft-lb
ASTM D5420
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
93.3
°C
200
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
54.4
°C
130
°F
ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
188
-
216
°C
370
-
420
°F
Middle Barrel Temperature
193
-
221
°C
380
-
430
°F
Front Barrel Temperature
199
-
227
°C
390
-
440
°F
Nozzle Temperature
204
-
216
°C
400
-
420
°F
Mold Temperature
26.7
-
48.9
°C
80.0
-
120
°F
Drying Temperature
65.6
-
82.2
°C
150
-
180
°F
Dry Time
1
-
2
hour
1
-
2
hour
Moisture Content
<= 0.050 %
<= 0.050 %
Recommended
Injection Pressure
2.76
-
10.3
MPa
400
-
1500
psi
Hold Pressure
2.07
-
8.27
MPa
300
-
1200
psi
Back Pressure
0.345
-
1.03
MPa
50.0
-
150
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LyondellBasell Sequel 1823-UV 9F42 Thermoplastic Olefinic Elastomer
PRHET285 / 65853
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.