MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chengdu Polyster KP-200H Silicone Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Silicone

Material Notes: KP-200 series silicone masterbatches are white pellets or white powder which made from ultra-high molecular weight polysiloxane, used by plastics as processing aids and impart expected silicone benefits to plastics, often more efficiently and more effectively than lower molecular weight silicone fluids, such as safety, little effect on the adhesion of paints, labels or decorations, more convenient to handle, good dispersion. Silicone masterbatches are with the carrier of polyethylene. For KP-200-30 silicone masterbatch, the content of siloxane is 30%. For KP-200-40 silicone masterbatch, the content of siloxane is 40%. For KP-200-50 silicone masterbatch, the content of siloxane is 50%. KP-200H silicone masterbatch is 100% pure silicone powder. KP-200 silicone masterbatch is with special silicon powder carrier, the content of silicone with ultra-high molecular weight is 50%.

Information provided by Chengdu Polyster Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
GB/T 3682
 
Component Elements PropertiesMetricEnglishComments
Silicon, Si 50 %50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 55279R028 Silicone Rubber/Fiberglass Laminate
Overview of materials for Silicone Elastomer, for Thermal Management
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
Chengdu Polyster KP-200-50 Silicone Masterbatch
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone

PCHEN022 / 79319

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.