MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic Grade HT250 Composite Material
Categories: Other Engineering Material

Material Notes:
  • High Hot Compressive Strength
  • Low Thermal Conductivity
  • Oil and Moisture Resistant
  • Reduces Heat Loss
  • Helps Control Temperature
  • Faster Mold Startup
Grade HT250 is a high compressive strength, heat-resistant composite material. Finished to a close thickness tolerance, it is ideal for insulation between the fold and the press or within the mold itself. It is completely asbestos-free and rugged to withstand rough handling during installation. It is easily cut and chained with standard metal working equipment. Diamond cutting tools are recommended for long life.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 300 MPa43500 psiASTM D790
Compressive Strength  450 MPa
@Temperature 180 °C
65200 psi
@Temperature 356 °F
ASTM D695
 600 MPa
@Temperature 23.0 °C
87000 psi
@Temperature 73.4 °F
ASTM D695
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 12.0 kV/mm305 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 µm/m-°C7.22 µin/in-°FAcross Surface; ASTM D696
 116 µm/m-°C64.4 µin/in-°FAcross Thickness; ASTM D696
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 250 °C482 °FContinuous
 400 °C752 °FMax
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling GLASTHERM HT250 Insulation Sheet
Gray Cast Iron, ASTM A 48 Class 40

PROCH9385 / 233087

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.