MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A213 T9 9Cr-1Mo STEEL TUBES FOR BOILERS AND HEAT EXCHANGERS (STBA 26)
Categories: Metal; Ferrous Metal; ASTM Steel; Stainless Steel; Cast Stainless Steel; Tool Steel; Cold Work Steel

Material Notes:

Creep and rupture data provided by NIMS

Key Words: JIS G3462 STBA 26; BS 3059-P2 622-490; ISO 2604 II S38; UNS K90941
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 415 MPa60200 psi
Tensile Strength, Yield 205 MPa29700 psi
Elongation at Break 30 %30 %
Rupture Strength  25.0 MPa
@Temperature 650 °C,
Time 3.60e+8 sec
3630 psi
@Temperature 1200 °F,
Time 100000 hour
 27.0 - 35.0 MPa
@Temperature 625 °C,
Time 3.60e+8 sec
3920 - 5080 psi
@Temperature 1160 °F,
Time 100000 hour
 39.0 - 46.0 MPa
@Temperature 600 °C,
Time 3.60e+8 sec
5660 - 6670 psi
@Temperature 1110 °F,
Time 100000 hour
 51.0 - 62.0 MPa
@Temperature 575 °C,
Time 3.60e+8 sec
7400 - 8990 psi
@Temperature 1070 °F,
Time 100000 hour
 66.0 - 81.0 MPa
@Temperature 550 °C,
Time 3.60e+8 sec
9570 - 11700 psi
@Temperature 1020 °F,
Time 100000 hour
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 8.0 - 10 %8.0 - 10 %
Iron, Fe 87.1 - 90.55 %87.1 - 90.55 %
Manganese, Mn 0.30 - 0.60 %0.30 - 0.60 %
Molybdenum, Mo 0.90 - 1.1 %0.90 - 1.1 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 0.25 - 1.0 %0.25 - 1.0 %
Sulfur, S <= 0.025 %<= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A213 T22 2.25Cr-1Mo STEEL FOR BOILER AND HEAT EXCHANGER SEAMLESS TUBES (STBA 24)
ASTM A213 T11 Alloy Steel, Chromium Molybdenum, F11-1
ASTM A213 T5 5Cr-0.5Mo STEEL TUBES FOR BOILERS AND HEAT EXCHANGERS (STBA 25)
321 Stainless Steel, annealed plate
AISI 4012 Steel

NIMS017 / 77534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.