MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV 24815 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24815 is a very low durometer thermoplastic vulcanizate designed for industrial applications requiring UV resistance. This grade is a low hardness, low density, lubricated grade suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Light Stabilized; Low Density; Low Hardness; Low Specific Gravity; Lubricated; Medium Flow; Slip

Uses: Expansion Joint; Gaskets; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  16
@Time 5.00 sec
16
@Time 0.00139 hour
Injection Molded; ASTM D2240
 22
@Time 1.00 sec
22
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 1.59 MPa230 psiFlow, Die C, 20 in/min; ASTM D412
 1.93 MPa280 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  0.455 MPa
@Strain 100 %
66.0 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 0.462 MPa
@Strain 100 %
67.0 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 1.28 MPa
@Strain 300 %
185 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
 1.30 MPa
@Strain 300 %
189 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 380 %380 %Flow, Die C, 20 in/min; ASTM D412
 420 %420 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 7.01 kN/m40.0 pliFlow, Die C, 20 in/min; ASTM D624
 7.54 kN/m43.0 pliAcross Flow, Die C, 20 in/min; ASTM D624
Compression Set  9.5 %
@Temperature 22.8 °C,
Time 79200 sec
9.5 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395
 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FInjection, Melt
Rear Barrel Temperature 173 - 213 °C344 - 416 °FInjection
Middle Barrel Temperature 179 - 219 °C354 - 426 °FInjection
Front Barrel Temperature 184 - 224 °C364 - 436 °FInjection
Nozzle Temperature 190 - 230 °C374 - 446 °FInjection
Zone 1 166 - 204 °C330 - 400 °FExtrusion
Zone 2 171 - 210 °C340 - 410 °FExtrusion
Zone 3 177 - 216 °C350 - 420 °FExtrusion
Zone 4 179 - 218 °C355 - 425 °FExtrusion
Zone 5 182 - 221 °C360 - 430 °FExtrusion
Die Temperature 190 - 227 °C374 - 440 °FExtrusion
Mold Temperature 35.0 - 60.0 °C95.0 - 140 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow XIAMETER™ RBL-2004-20 LSR Liquid Silicone Rubber
Wacker Elastosil® LR 3003/20 TR A/B Liquid Silicone Rubber
RTP Company RTP 2720 S-30A Saturated Styrenic Block Copolymer
Teknor Apex Medalist® MD-110 Thermoplastic Elastomer
Avient Versaflex™ CL30 Thermoplastic Elastomer (TPE)

PTEKNQ1196 / 237687

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.