Property data below is typical of annealed samples. Available in plate. For use in fasteners, military equipment and air frame parts. Information provided by Allegheny Ludlum |
DIN 1.4545; ASTM A693; ASME SA693; AMS 5562, 15-5PH, 15-5 PH, 15/5PH, 15/5 PH, Precipitation Hardening |