Covestro Desmopan® 2384A GMP TPU
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Extrusion grade; does not contain any anti-hydrolysis agent; Beads; Application; Films; Hoses, non-reinforced
Mechanical property data for samples at 50% RH.
Information provided by Covestro
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
83
83
ISO 868
Tensile Strength, Ultimate
44.0
MPa
6380
psi
200 mm/min; DIN 53504
Elongation at Break
681 %
681 %
200 mm/min; DIN 53504
Tensile Modulus
0.0150
GPa
@Temperature 60.0 °C
2.18
ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
0.0260
GPa
@Temperature 20.0 °C
3.77
ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
0.443
GPa
@Temperature -20.0 °C
64.3
ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
50% Modulus
4.30
MPa
@Strain 50 %
4.30
MPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus
5.50
MPa
@Strain 100 %
798
psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus
10.4
MPa
@Strain 200 %
1510
psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound
46 %
46 %
Resilience; ISO 4662
Tear Strength
65.0
kN/m
371
pli
500 mm/min; ISO 34-1
Abrasion
39
39
mm3; ISO 4649 method A
Compression Set
24 %
@Temperature 70.0 °C,
Time 86400 sec
24 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
58 %
@Temperature 23.0 °C,
Time 259000 sec
58 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
Processing Properties
Metric
English
Comments
Melt Temperature
190
-
210
°C
374
-
410
°F
Extrusion
190
-
220
°C
374
-
428
°F
Injection
Mold Temperature
20.0
-
40.0
°C
68.0
-
104
°F
Drying Temperature
90.0
°C
194
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Covestro Desmopan® 1080AU TPU
Covestro Desmopan® 1085A TPU
Covestro Desmopan® 2792A GMP TPU
Covestro Desmopan® 453 DPS 041 TPU
Covestro Desmopan® 9392A GMP TPU
PCOVEST0691 / 202474
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.