MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Outokumpu 4310 Cr-Ni Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.

Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.431; ASTM 301; JIS SUS 301
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 800 MPa116000 psiOutokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Tensile Strength, Yield  250 MPa
@Strain 0.2 %
36300 psi
@Strain 0.2 %
EN min., RT; EN 10002-1
 300 MPa
@Strain 0.2 %
43500 psi
@Strain 0.2 %
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
 330 MPa
@Strain 1 %
47900 psi
@Strain 1 %
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
 190 MPa
@Strain 0.2 %,
Temperature 200 °C
27600 psi
@Strain 0.2 %,
Temperature 392 °F
EN min.; EN 10002-5
 210 MPa
@Strain 0.2 %,
Temperature 100 °C
30500 psi
@Strain 0.2 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 50 %50 %Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Modulus of Elasticity 200 GPa29000 ksiRT
 172 GPa
@Temperature 400 °C
24900 ksi
@Temperature 752 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000730 ohm-cm0.0000730 ohm-cmRT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.0 µm/m-°C
@Temperature 100 °C
8.89 µin/in-°F
@Temperature 212 °F
 18.0 µm/m-°C
@Temperature 400 °C
10.0 µin/in-°F
@Temperature 752 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°FRT
Thermal Conductivity 15.0 W/m-K104 BTU-in/hr-ft²-°FRT
 20.0 W/m-K
@Temperature 400 °C
139 BTU-in/hr-ft²-°F
@Temperature 752 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.10 %0.10 %
Chromium, Cr 17 %17 %
Iron, Fe 75.9 %75.9 %
Nickel, Ni 7.0 %7.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
301 Stainless Steel
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
AK Steel 301 Austenitic Stainless steel
304 Stainless Steel

NOUTOK09 / 18724

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.