MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Buckeye Polymers BP RPP 2007 TR Blk Reprocessed Polypropylene, 20% Mineral Filled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Talc Filled Black

This reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds are utilized in this mineral reinforced polypropylene product to help meet the wide recycling requirements.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
Melt Flow 7.0 g/10 min7.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 27.6 MPa4000 psiASTM D638
Flexural Modulus 2.10 GPa305 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C225 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell RA-14 Copolymer Polypropylene, 20% Talc Filled
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled
LG Chemical LUPOL HM5204 PP+MF20%, High Impact
LyondellBasell Hostacom BR 735 G 3169 Polypropylene, Mineral Reinforced
MTM Plastics Dipolen® SL Recycled LDPE Blend

PBUK35 / 27890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.