MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Linear Mold Shrinkage 0.014 - 0.019 cm/cm0.014 - 0.019 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.8 MPa6500 psiASTM D638
Elongation at Yield 50 %50 %ASTM D638
Flexural Yield Strength 55.2 MPa8000 psiASTM D790
Flexural Modulus 1.59 GPa230 ksiASTM D790
Izod Impact, Notched 8.28 J/cm
@Temperature 22.8 °C
15.5 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C160 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 266 - 288 °C510 - 550 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Dry Time 2 - 4 hour
@Temperature 79.4 °C
2 - 4 hour
@Temperature 175 °F
to ensure moisture content is less than 0.2%
Injection Pressure 4.96 - 8.27 MPa720 - 1200 psiSecondary
 8.27 - 13.8 MPa1200 - 2000 psiInitial
Back Pressure 0.345 - 1.72 MPa50.0 - 250 psi
Shot Size 30 - 80 %30 - 80 %
Screw Speed 20 - 100 rpm20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated
Clariant Renol PA223G13 Nylon 6, 13% Glass Fiber, Impact Modified
Clariant Renol PA1SP0005 Nylon 66, Impact Modified, Glass Reinforced
Clariant Renol PA1SP0004 Nylon 66, High Impact Modified, ESD
Clariant Renol PA123G13 Nylon 66, 13% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated

PCLAR031 / 82156

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.