MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Oroglas® HFI-10 Acrylic, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.

Key features :

  • impact resistance: up to 10 times more impact-resistant than standard acrylic
  • easy processing: flow significantly improved which contribute to reduce cycle time by 20 %.

( MFI, 230°c/3.8 kg ) = 3 gr / 10 min ( MVI, 230°c/3.8 kg ) = 2.8 ml / 10 min

  • excellent optical properties with low edge color
  • UV stability

Typical applications :
OROGLAS HFI-10 can be injection molded or extruded in any type of machine Typical applications are in the fields of: building, lighting, appliances, information technology, and business machines. OROGLAS HFI-10 is recommended when toughness and increased flow are required.

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Water Absorption 2.0 %2.0 %
Moisture Absorption at Equilibrium 0.36 %0.36 %Humidity Absorption
Melt Flow 2.8 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.8 g/10 min
@Load 8.38 lb,
Temperature 446 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psi50 mm/min
Elongation at Break 30 %30 %Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %5.0 %50 mm/min
Tensile Modulus 1.70 GPa247 ksi1 mm/min
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²
Tensile Creep Modulus, 1 hour 1400 MPa203000 psi
Tensile Creep Modulus, 1000 hours 1000 MPa145000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
Dielectric Strength 15.0 kV/mm381 kV/in
Dissipation Factor  0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
 0.050
@Frequency 100 Hz
0.050
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature 20.0 °C
55.6 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °F
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °F
Vicat Softening Point 84.0 °C183 °F50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %Mfr. reports 'Transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Plexiglas® SG10 Acrylic
Arkema Oroglas® HFI-7 Acrylic
Celanese Hostaform® MT® SlideX™ 1203 POM, Medical Technology
Celanese Hostaform® MT® SlideX™ 2404 POM, Medical Technology
Arkema Oroglas® DRT Acrylic, Impact Grade

PZARKG488 / 25746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.