MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Agricultural Film
  • Co-Extrusion Films
  • Foams
  • Form Fill and Seal Packaging
  • Freezer Film
  • High Clarity Film
  • Lamination Film
  • Poultry Bag
  • Rice Bags
  • Rubber Bale Wrap

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³ExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 220 %220 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Elmendorf Tear Strength MD 170 g170 gASTM D1922
Elmendorf Tear Strength TD 60 g60 gASTM D1922
Dart Drop Test 150 g0.331 lbASTM D1709A
Film Tensile Strength at Break, MD 32.4 MPa4700 psiASTM D882
Film Tensile Strength at Break, TD 18.6 MPa2700 psiASTM D882
1% Secant Modulus, MD 172 MPa25000 psiASTM D882
1% Secant Modulus, TD 200 MPa29000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 °C219 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 6.9 %6.9 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 1881 Polycarbonate
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin

PEX99245 / 175481

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.