MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® K224-G0 PA6-GF50, Dry, 50% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: 50% Glass Reinforced

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183
Water Absorption 4.5 %4.5 %Sim. ISO 62
Moisture Absorption 1.40 %1.40 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0033 cm/cm0.0033 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0076 cm/cm0.0076 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 220 MPa31900 psiISO 527-1/-2
Elongation at Break 3.0 %3.0 %ISO 527-1/-2
Tensile Modulus 16.5 GPa2390 ksiISO 527-1/-2
Flexural Strength 310 MPa45000 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Charpy Impact Unnotched  9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60250
Dielectric Constant  3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
IEC 60250
 5.2
@Frequency 1e+6 Hz
5.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
IEC 60695-11-10
Glow Wire Ignition Temperature  725 °C
@Thickness 2.00 mm
1340 °F
@Thickness 0.0787 in
IEC 60695-2-13
 725 °C
@Thickness 1.50 mm
1340 °F
@Thickness 0.0591 in
IEC 60695-2-13
Glow Wire Flammability Index  700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-12
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® K224-G0 PA6-GF50, Conditioned, 50% Glass Filled
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned)
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled
Techmer ES HiFill® PA6 GF50 50% Glass Filled
Envalior Akulon® K224-G6 PA6-GF30, Conditioned, 30% Glass Filled

PDSM8027 / 184728

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.