MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech PP7110 Talc Filled High Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain critical

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc
@Temperature 22.8 °C
0.960 g/cc
@Temperature 73.0 °F
ASTM D792
Filler Content 10 %10 %
Linear Mold Shrinkage 0.018 cm/cm0.018 in/in0.125inch wall
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.1 MPa3200 psiASTM D638
Elongation at Break >= 400 %>= 400 %ASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus 1.10 GPa160 ksisecant; ASTM D790
 1.38 GPa200 ksitangent; ASTM D790
Izod Impact, Notched >= 5.34 J/cm
@Temperature 22.8 °C
>= 10.0 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact >= 33.9 J
@Temperature 22.8 °C
>= 25.0 ft-lb
@Temperature 73.0 °F
ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C195 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.1 °C115 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 55 %55 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Spartech PP5140 Talc Filled Homopolymer
Spartech PP5130 Talc Filled Homopolymer
Spartech PP5110 Talc Filled Homopolymer
Spartech PP7140 Talc Filled High Impact Copolymer
Spartech PP5210 Calcium Carbonate Filled Homopolymer

PSPAR101 / 78723

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.