MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Novaduran® 5010G15 Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Standard. 15 %GF reinforced UL-HB grade. Excellent mechanical properties. Excellent heat resistance. Excellent moldability and flowability. Low moisture absorption rate for high dimensional stability. Excellent surface gloss and color. Excellent oil and chemical resistance. Excellent electrical properties. Excellent friction and abrasion resistance. Flame retardant grades also available.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Water Absorption 0.080 %
@Temperature 23.0 °C
0.080 %
@Temperature 73.4 °F
Immersion
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
100 mm long x 100 mm wide
Linear Mold Shrinkage, Transverse 0.013 cm/cm
@Thickness 2.00 mm
0.013 in/in
@Thickness 0.0787 in
100 mm long x 100 mm wide
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiISO 527-1,2
Elongation at Break 3.0 %3.0 %ISO 527-1,2
Tensile Modulus 5.80 GPa841 ksiISO 527-1,2
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 5.50 GPa798 ksiISO 178
Charpy Impact Unnotched 2.40 J/cm²11.4 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+16 ohm-cm5.00e+16 ohm-cmIEC 60093
Surface Resistance 4.00e+16 ohm4.00e+16 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength  21.0 kV/mm
@Thickness 2.00 mm
533 kV/in
@Thickness 0.0787 in
IEC 60243-1
 24.0 kV/mm
@Thickness 1.00 mm
610 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  30.0 µm/m-°C
@Temperature -30.0 - 120 °C
16.7 µin/in-°F
@Temperature -22.0 - 248 °F
ISO 11359-2
 30.0 µm/m-°C
@Temperature -30.0 - 50.0 °C
16.7 µin/in-°F
@Temperature -22.0 - 122 °F
ISO 11359-2
 30.0 µm/m-°C
@Temperature 50.0 - 120 °C
16.7 µin/in-°F
@Temperature 122 - 248 °F
ISO 11359-2
CTE, linear, Transverse to Flow  90.0 µm/m-°C
@Temperature -30.0 - 50.0 °C
50.0 µin/in-°F
@Temperature -22.0 - 122 °F
ISO 11359-2
 120 µm/m-°C
@Temperature -30.0 - 120 °C
66.7 µin/in-°F
@Temperature -22.0 - 248 °F
ISO 11359-2
 140 µm/m-°C
@Temperature 50.0 - 120 °C
77.8 µin/in-°F
@Temperature 122 - 248 °F
ISO 11359-2
Melting Point 224 °C435 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 198 °C388 °FISO 75-1,2
Flammability, UL94 HB
@Thickness 0.840 mm
HB
@Thickness 0.0331 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gromax CCP PBT 3010-104 10% Glass Fiber Filled
Evonik Vestodur® GF 50 50% Glass Reinforced PBT
Envalior Pocan® B 4215 000000 PBT, 12% Glass Fiber
Celanese Celanex® 3214 15% Fiberglass Reinforced Polybutylene Terephthalate
BASF Ultradur® B 4300 G2 BK5110 10% Glass Filled PBT

PMITSU9055 / 191728

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.