MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 10% Cold Rolled (UNS S30500)
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to corrosion, prevention of product contamination, resistance to oxidation, ease of fabrication, excellent formability, beauty of appearance, ease of cleaning, high strength with low weight, good strength and toughness at cryogenic temperatures, and readily availability of a wide range of product forms. Food and beverage, sanitary, cryogenic, and pressure-containing applications are examples. Type 305 is used for applications requiring a low rate of work hardening during severe cold forming operations such as deep drawing.

Information provided by Allegheny Ludlum Corporation.

Key Words: Plate, sheet, and strip specs: ASTM A 240; ASME SA-240
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.90 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8888
Tensile Strength, Ultimate 648 MPa94000 psi
Tensile Strength, Yield 517 MPa75000 psi
Elongation at Break 45 %45 %
Tensile Modulus 200 GPa29000 ksi
Charpy Impact 200 J148 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
Magnetic Permeability 1.0031.00310% cold work
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.6 µm/m-°C
@Temperature 20.0 - 100 °C
9.22 µin/in-°F
@Temperature 68.0 - 212 °F
 19.8 µm/m-°C
@Temperature 20.0 - 870 °C
11.0 µin/in-°F
@Temperature 68.0 - 1600 °F
Specific Heat Capacity 0.500 J/g-°C0.120 BTU/lb-°F
Thermal Conductivity  16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.4 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1399 - 1421 °C2550 - 2590 °F
Solidus 1399 °C2550 °F
Liquidus 1421 °C2590 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 17 - 19 %17 - 19 %
Iron, Fe 69 %69 %as balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 10.5 - 13 %10.5 - 13 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
ATI Allegheny Ludlum Grade 3 Titanium (UNS R50550)
ATI Allvac® Nickelvac® H-W Nickel Superalloy, Heat Treatment: 1185°C (2165°F) Anneal
Special Metals Nickel 200
Haynes Hastelloy® B-2 alloy, plate, 9.1-51 mm thick, heat treated at 1066°C, rapid quenched

NL3051 / 17867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.