MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zoltek™ OX FT0500-200 Oxidized PAN Fiber Felt
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Produced from 100% ZOLTEK OX oxidized PAN fibers, needlepunched felts are for use as thermal/acoustical insulation in aerospace, automotive or general industrial high temperature applications. Valuable as a low cost - high performance fire or spark barrier.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
Thickness 4200 microns165 milCured
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 8.00e+8 ohm-cm8.00e+8 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Oxygen Index >= 40 %>= 40 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 62 %62 %
Hydrogen, H 4.5 %4.5 %
Nitrogen, N 21.5 %21.5 %
O2 12 %12 %
Sodium, Na <= 0.10 %<= 0.10 %
Trace Metals <= 0.010 %<= 0.010 %
 
Descriptive Properties
Areal Weight500 g/m2. (custom weights available)
ColorBlack
Fiber Diameter (µm)12.5
Fiber Input1.7 or 2.2 dTex.
Organic SolventsExcellent resistance
Roll Length100m
Roll Width203 cm.
Strong AcidsGood resistance
Strong BasesPoor resistance
Weak AcidsExcellent resistance
Weak BasesGood resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 Type-55 Chopped Carbon Fiber
Zoltek™ PX35 Type-02 Chopped Carbon Fiber
A-Glass Fiber, Generic
E-Glass Fiber, Generic
Hexcel® HexTow® AS4C 6K Standard Modulus Carbon Fiber (6000 Filaments)

ECZO832 / 232304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.