MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Features

PA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, CTI 300. Application for the electrical industry: protectors, coil forms, covers, terminals. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0058 cm/cm0.0058 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0137 cm/cm0.0137 in/inSTN 64 0808
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiSTN EN ISO 527-2
Elongation at Break 2.0 %2.0 %STN EN ISO 527-2
Tensile Modulus 4.20 GPa609 ksiSTN EN ISO 527-2
Flexural Strength 120 MPa17400 psiSTN EN ISO 178
Flexural Modulus 3.50 GPa508 ksiSTN EN ISO 178
Charpy Impact Unnotched  1.50 J/cm²
@Temperature -20.0 °C
7.14 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.100 J/cm²
@Temperature 23.0 °C
0.476 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 0.100 J/cm²
@Temperature -20.0 °C
0.476 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FSTN EN ISO 75/A
Vicat Softening Point 200 °C392 °FB; STN EN ISO 306
Flammability, UL94 V-0V-0
Glow Wire Test 960 °C1760 °FSTN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 205 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant
RTP Company RTP 204 A FR UV Nylon 6 (PA), Glass Fiber - Flame Retardant - UV Stabilized
RTP Company RTP 204 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant
RTP Company RTP 203 A FR UV Nylon 6 (PA), Glass Fiber - Flame Retardant - UV Stabilized - UL94 V-0
RTP Company RTP 203 A FR Nylon 6 (PA), Glass Fiber - Flame Retardant

PPLACO026 / 106904

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.